The short answerRun PETG hot, and keep the bed warm.

A PETG nozzle sits between 240 and 260 °C, and the bed lands near 80 °C. The Prusament and Polymaker datasheets set those bands. Start in the middle and tune for stringing or warping.

The nozzle range

PETG melts higher than PLA. The Prusament PETG datasheet lists 250 °C with a 10 °C margin, and the Polymaker PETG sheet lists 240 to 260 °C. Stay inside that band. Below 240 °C the layers bond weakly. Above 260 °C the filament strings and oozes.

PETG print temperature
SettingRecommendedWhy
Nozzle temperature240 to 260 °CPrusament 250 ±10, Polymaker 240 to 260.
Bed temperature70 to 80 °CPrusament lists 80 °C with a 10 °C margin.
Part cooling fan20 to 60 %Keep fan low for the first layers.
Print speed40 to 60 mm/sSlow down for clean corners.

Bed temperature

Prusament sets the PETG bed at 80 °C with a 10 °C margin. Polymaker lists 60 to 70 °C for the build plate. A bed of 70 to 80 °C sits inside both. Drop to 60 °C if the part prints too hot and lifts at the center.

Tuning for common flaws

PETG temperature tuning
Likely causeFixSeverity
Stringing between movesDrop the nozzle 5 °C and add retractionmd
Corners liftingRaise the bed to 80 to 90 °C and clean the sheethi
Weak layer adhesionRaise the nozzle 5 °C toward 260 °Cmd
Rough top surfaceSlow the print speed to 40 mm/slo

Key takeaways

  • Print PETG at 240 to 260 °C on the nozzle.
  • Set the bed to 70 to 80 °C, or up to 90 °C if corners lift.
  • Keep the part cooling fan between 20 and 60 %.
  • Dry wet PETG before you blame the temperature.

Frequently asked

What temperature should I set my PETG nozzle to?
Start at 250 °C. The Prusament and Polymaker ranges run 240 to 260 °C. Tune down for stringing and up for weak layers.
Is 60 °C too low for a PETG bed?
It is the low edge. Polymaker lists 60 to 70 °C. Use 60 °C only if 80 °C prints too hot, and watch for lifting.
Why does my PETG string at the right temperature?
The filament is probably wet, or the retraction is too low. Dry the PETG first, then tune retraction.
Do I need a temperature tower for PETG?
It helps. Print a tower from 240 to 260 °C and pick the band with the cleanest stringing and best layer adhesion.

For the full settings set, read the PETG temperature guide. For the broader material overview, see the PETG filament page. Stringing that does not clear with temperature usually needs the PETG retraction settings.

Related guides

Sources & methodology

5 citations · reviewed 2026-07-09
  1. 01Prusament PETG Technical Datasheetaccessed 2026-07-06Tier 1
  2. 02Polymaker PETG Technical Data Sheetaccessed 2026-07-06Tier 1
  3. 03Bambu Lab PETG Usage Guideaccessed 2026-06-29Tier 1
  4. 043DSourced PETG Filament Guideaccessed 2026-06-29Tier 2
  5. 05All3DP PETG Comprehensive Guideaccessed 2026-06-30Tier 2
How we vetted this: every claim traces to a tiered source, Tier 1 (manufacturer, slicer, standards) first. Read the full sourcing and conflict-of-interest policy.